Effect of Work-Hardening Mechanisms in Asymmetrically Cyclic-Loaded Austenitic Stainless Steels on Low-Cycle and High-Cycle Fatigue Behavior

Moshtaghi, Masoud & Safyari, Mahdieh. (2021). Effect of Work Hardening Mechanisms in Asymmetrically Cyclic Loaded Austenitic Stainless Steels on Low‐Cycle and High‐Cycle Fatigue Behavior. Steel Research International. 92. 10.1002/srin.202000242.

Related Products: EHF Series Fatigue Testing Systems

Read/Download 

 

Experimental Study on Improving the Mechanical Properties of Material Extrusion Rapid Prototyping Polylactic Acid Parts by Applied Vibration

YJiang, Shijie, Tiankuo Dong, Yang Zhan, Weibing Dai, and Ming Zhan. 2021. "Experimental Study on Improving the Mechanical Properties of Material Extrusion Rapid Prototyping Polylactic Acid Parts by Applied Vibration" Applied Sciences 11, no. 4: 1820. https://doi.org/10.3390/app11041820

Related Products: EHF Series Fatigue Testing Systems

Read/Download 

 

Local strain measurement in tensile test of Al/steel dissimilar friction stir weld using digital image correlation

Yoshihiko Uematsu, Toshifumi Kakiuchi, Kenta Niimi, Paul Dario Toasa Caiza DOI: https://doi.org/10.21203/rs.3.rs-421146/v1

Related Products: EHF Series Fatigue Testing Systems

Read/Download 

 

Crack initiation and propagation mechanisms of an extruded dual-phase Magnesium-Lithium alloy in very high cycle fatigue regime

iangyu WANG, Chao HE, Xue LI, et al. Crack initiation and propagation mechanisms of an extruded dual-phase Magnesium-Lithium alloy in very high cycle fatigue regime. Authorea. April 27, 2021.

Related Products: USF-2000A

Read/Download 

 

Critical Dynamics of Defects and Mechanisms of Damage-Failure Transitions in Fatigue

Naimark, O.; Oborin, V.; Bannikov, M.; Ledon, D. Critical Dynamics of Defects and Mechanisms of Damage-Failure Transitions in Fatigue. Materials 2021, 14, 2554. https://doi.org/10.3390/ma14102554

Related Products: USF-2000A

Read/Download 

 

Investigation of S275JR+AR structural steel fatigue performance in very high cycle domain

Gorash, Yevgen & Comlekci, Tugrul & Styger, Gary & Kelly, James & Brownlie, Frazer. (2021). Investigation of S275JR+AR structural steel fatigue performance in very high cycle domain.

Related Products: USF-2000A, Universal/Tensile Test Frames

Read/Download 

 

Improvement on the mechanical properties of eutectic Sn58Bi alloy with porous Cu addition during isothermal aging

Improvement on the mechanical properties of eutectic Sn58Bi alloy with porous Cu addition during isothermal aging To cite this article before publication: Yang Liu et al 2021 Mater. Res. Express in press https://doi.org/10.1088/2053-1591/ac10d5

Read/Download 

 

Critical Dynamics of Defects and Mechanisms of Damage-Failure Transitions in Fatigue

Naimark, O.; Oborin, V.; Bannikov, M.; Ledon, D. Critical Dynamics of Defects and Mechanisms of Damage-Failure Transitions in Fatigue. Materials 202114, 2554. https://doi.org/10.3390/ma14102554

Read/Download 

 

Micro-Brazing of Stainless Steel Using Ni-P Alloy Plating

Liu, S.; Shohji, I.; Iioka, M.; Hashimoto, A.; Hirohashi, J.; Wake, T.; Arai, S. Micro-Brazing of Stainless Steel Using Ni-P Alloy Plating. Appl. Sci. 2019, 9, 1094. https://doi.org/10.3390/app9061094

Read/Download 

 

Single edge crack fracture behavior of S2 glass/epoxy under different temperature, strain rate and crack length

Kaya, Zafer & Balcıoğlu, H. & Gun, Halit. (2021). Single edge crack fracture behavior of S2 glass/epoxy under different temperature, strain rate and crack length. Research on Engineering Structures and Materials. 10.17515/resm2021.263me0219. 