Rechargeable Lithium-Ion Battery Evaluation

The lithium-ion rechargeable battery is a relatively new type of battery that was first used in the early 1990s. With their high voltage and high energy density, these batteries are widely used for consumer electronics applications, such as mobile phones and laptop computers. Due to enhanced consumer concerns for the environment and fuel savings, the automobile industry has also been developing these batteries for hybrid vehicle (HV) and electric vehicle (EV) applications, which should lead to enhanced output, efficiency, and performance. As a leading manufacturer of a broad range of analytical and testing instruments, Shimadzu provides a variety of solutions that contribute to research, development, and quality control of lithium-ion rechargeable batteries as they become more widely used in consumer electronics and eco-cars.

Content Type:
Analysis Guidebook
Document Number:
C10G-E021A
Product Type:
Material Testing, Universal / Tensile Testing
Keywords:
Materials/Automotive, Batteries & Fuel Cells
Language:
English
File Name:
c10g-e021a.pdf
File Size:
3,752kb

View Article

Top of This Page