Analysis of Dimethicone Based on USP-Specified Method

Viscous dimethicone samples were analyzed by ATR spectroscopy, and excellent repeatability was obtained.Quantitative analysis by the solution method has the advantage of high sensitivity with the ability to detect low-level absorption through appropriate selection of a solid cell. However, for analysis of samples having some degree of viscosity, as those presented here, the ATR method with its simple measurement and easy cleaning of the prism, is very effective.