High-Speed Monitoring of Curing Reaction in UV-Irradiated Resin by Rapid Scan

Here, us ing the ShimadzuIRTracer-100 FTIR spectrophotometer Rapid Scanfeature, we introduce the results of measurement ofthe curing reaction process that occurs in UV-curableresin.