RF-6000 Application - Fluorescence Measurement of Organic Electroluminescent Material

As the development of various organic EL materialscontinues, there will be a demand for spectra of highersensitivity over a broader wavelength range to use inorganic EL material evaluation. The RF-6000 is able toacquire 3D spectra quickly and accurately, andsimultaneously acquire spectra with high sensitivity upto 900 nm. Using an optional integrating sphere withthe RF-6000 also allows the measurement of quantumefficiency (absolute quantum yield).In this study, using the RF-6000 spectrofluorophotometer,we successfully verified the 3D spectra and fluorescencespectra of an organic EL material.

Content Type:
Application News
Document Number:
LAAN-A-RF-E010
Product Type:
Molecular Spectroscopy, Fluorescence Spectroscopy
Keywords:
Electronics, Ceramics, Metals, Mining, Materials/Automotive
Language:
English
File Name:
eA516 - Fluorescence Measurement of Organic Electroluminescent Material.pdf
File Size:
96kb