Measuring of Coating Additives

Coatings are an ideal protection for different kind of materials. They protect against moisture, UV radiation, rust and other influences. Additives can enhance the properties of the coating, e.g. the scratch resistance. Like in this application note these additives can be made out of non-polar surface modified silicon dioxide nanoparticles.