Tensile Testing of Carbon Fiber

Carbon fiber is an important industrial material, being essential in carbon fiber reinforced plastics (CFRP), having a specific gravity one-fourth that of normal steels, and a specific strength of 7 times. In this Application Data Sheet, examples of tensile testing of single carbon fibers based on the ISO standard are introduced.