Effect of Work-Hardening Mechanisms in Asymmetrically Cyclic-Loaded Austenitic Stainless Steels on Low-Cycle and High-Cycle Fatigue Behavior

Moshtaghi, Masoud & Safyari, Mahdieh. (2021). Effect of Work Hardening Mechanisms in Asymmetrically Cyclic Loaded Austenitic Stainless Steels on Low‐Cycle and High‐Cycle Fatigue Behavior. Steel Research International. 92. 10.1002/srin.202000242.

Related Industries: Metal and Alloy Materials Testing

Read/Download 

 

Experimental Study on Improving the Mechanical Properties of Material Extrusion Rapid Prototyping Polylactic Acid Parts by Applied Vibration

YJiang, Shijie, Tiankuo Dong, Yang Zhan, Weibing Dai, and Ming Zhan. 2021. "Experimental Study on Improving the Mechanical Properties of Material Extrusion Rapid Prototyping Polylactic Acid Parts by Applied Vibration" Applied Sciences 11, no. 4: 1820. https://doi.org/10.3390/app11041820

Related Industries: Metal and Alloy Materials Testing

Read/Download 

 

Local strain measurement in tensile test of Al/steel dissimilar friction stir weld using digital image correlation

Yoshihiko Uematsu, Toshifumi Kakiuchi, Kenta Niimi, Paul Dario Toasa Caiza DOI: https://doi.org/10.21203/rs.3.rs-421146/v1

Related Industries: Metal and Alloy Materials Testing

Read/Download 

 

Crack initiation and propagation mechanisms of an extruded dual-phase Magnesium-Lithium alloy in very high cycle fatigue regime

iangyu WANG, Chao HE, Xue LI, et al. Crack initiation and propagation mechanisms of an extruded dual-phase Magnesium-Lithium alloy in very high cycle fatigue regime. Authorea. April 27, 2021.

Related Industries: Metal and Alloy Materials Testing

Read/Download 

 

Critical Dynamics of Defects and Mechanisms of Damage-Failure Transitions in Fatigue

Naimark, O.; Oborin, V.; Bannikov, M.; Ledon, D. Critical Dynamics of Defects and Mechanisms of Damage-Failure Transitions in Fatigue. Materials 2021, 14, 2554. https://doi.org/10.3390/ma14102554

Related Industries: Metal and Alloy Materials Testing

Read/Download 

 

Investigation of S275JR+AR structural steel fatigue performance in very high cycle domain

Gorash, Yevgen & Comlekci, Tugrul & Styger, Gary & Kelly, James & Brownlie, Frazer. (2021). Investigation of S275JR+AR structural steel fatigue performance in very high cycle domain.

Related Industries: Metal and Alloy Materials Testing

Read/Download 

 
 