Dynamic Characteristics Testing Machine for Rubber Vibration Isolators

For Rubber Vibration Isolator Research and Development

Dynamic Characteristics Testing Machine for Rubber Vibration Isolators

This instrument can measure and process the data of spring constants, damping coefficients and loss factors of viscoelastic materials from static status to high cycles up to 300 MHz. The thermostatic chamber permits testing in controlled temperature environments.

Features

Specifications

Maximum Test Force ±10kN
Maximum Displacement ±10mm
Cycle Speed 5 to 300 Hz
Amplitude Characteristics 50Hz ±2mm ,100Hz ±0.9mm , 200Hz ±0.36mm , 300Hz ±0.18mm

Note: Contact Shimadzu for further details.