iSpect DIA-10 Dynamic Image Particle Size and Shape Analyzer

iSpect DIA-10 Dynamic Image Particle Size and Shape Analyzer

 
 

Specifications

Measurement Method Dynamic image analysis
Particle Size Measurement Range*1 5 to 100 µm
Number Concentration*2 Coefficient of Variation (CV) ≦ 5 %
Measurement Parameters

Size Parameters
Area Circle Equivalent Diameter, Perimeter Equivalent Diameter, Maximum Length, Maximum Perpendicular Length, Vertical Feret Diameter, Horizontal Feret Diameter, Particle Perimeter, Envelope Perimeter
Shape Parameters
Circularity, Aspect Ratio, Horizontal Bounding Rectangle Aspect Ratio
Other Parameters
Particle Area, Average Brightness

Statistical Analysis Parameters Average, standard deviation, CV, median, mode, user defined % value
Display Parameters Particle image, histogram, scatter plot, cumulative distribution, frequency/integration table, user defined area particle count
Sample Size 50 to 1000 µL
Pump Syringe pump, flowrate 0.1 mL/min
Measurement Unit Material PEEK resin, fluorine resin, quartz, fluorinated rubber
Pump Unit Material Fluorine resin, glass
Power Supply Requirements 100 V AC, 100 VA, 50/60 Hz
Dimensions/Weight Measurement unit: W223 × D465 × H205 mm, 10 kg
Pump unit: W97 × D190 × H150 mm, 3 kg
 
*1: Performance guarantee range of area circle equivalent diameter. Measured using a Shimadzu NIST traceable particle size standard sample.
*2: Measured using concentration standard samples specified by Shimadzu.