SALD-7500 Particle Size Analyzer

Tailored towards real-time, submicron particle characterization

SALD-7500 Particle Size Analyzer

Specifications

General Specifications

Measurement principle Laser Diffraction Method
Measurement range 7 nm (0.007 μm) to 800 μm (when using sampler)
7 nm (0.007 μm) to 400 μm (when using batch cell)
30 nm (0.03 μm) to 280 μm (when using high-concentration sample unit)

Note 1: The measurement range varies according to the shape etc. of the particle.

Measurement unit : SALD-7500nano

Measurement principle Laser Diffraction Method
Light source Semiconductor laser (Wavelength 405 nm)
Light detector Detector elements for violet semiconductor laser Total 84 elements (78 forward, 1 side, 5 back)
System Compliance Class 1 Laser Product, CE
Required power supply AC 100 V±10%, 1 A, 50/60 Hz
Dimensions & weight Approx. 680 × D280 × H430 mm, Approx.32 kg
Operation environment Temperature : 10 to 30°C , Humidity : 20 to 80% (no condensation)

Note 2: Reference sample and USB cable (2 m) supplied as standard
Note 3: Ultrasonic cleaning instruments are needed for the measurement of reference sample.

Sampler : SALD-MS75

Dispersing bath Capacity : 100 / 200 / 300 mL
Sonicator Frequency : about32 kHz, output : about 40 W
Liquid pump Radial pump, maximum flow rate 2000 cm3/min
Liquid pump material Stainless (SUS 304, SUS 316), Tetrafluoroethylene (PTFE), Perfluoroelastmor (FEP)
Liquid supply pump Diaphragm pump, maximum flow rate : 750cm3/min
Liquid supply pump material Polypropylene
Flow cell Quartz glass
Required power supply AC 100 V±10%, 2 A, 50/60 Hz
Dimensions & weight Approx. W390 × D520 × H430 mm, Approx.18 kg
Operating environment Temperature: 10 to 30°C, Humidity: 20 to 80% (no condensation)

Note 4: USB cable (2 m) supplied as standard

Batch Cell : SALD-BC75

Cell material Quartz glass
Required liquid volume Approx. 5 cm3
Stirrer mechanism Up-and-down movement of blade
Dimensions & weight Approx. W100 × D120 × H140 mm, Approx. 0.8 kg
Operating environment Temperature: 10 to 30°C, Humidity: 20 to 80% (no condensation)

High-concentration Sample Measurement System : SALD-HC75

Cell material Borosilicate glass
Required liquid volume Approx. 0.15 cm3
Dimensions & weight Approx. W20 × D100 × H9 mm, Approx. 0.2 kg
Operating environment Temperature: 10 to 30°C, Humidity: 20 to 80% (no condensation)

Software Specifications

(WingSALD II)

Measurement and Data Display Functions
Measurement of Particle Size Distribution Allows measurements using measurement assistant function (interactive process based on SOP)
Refractive Index Setting Automatic refractive index calculation function (LDR method: Light Intensity Distribution Reproduction Method) makes setting the refractive index easy.
Real-Time Display Particle size distribution/light intensity distribution simultaneous display
Diagnostics/Adjustments Self-diagnostic function and cell check function
Recalculation of Particle Size Distribution Batch recalculation of max. 200 distributions
Display of Particle Size Distribution Data Displays overlay of max. 200 distributions
Display of Light Intensity Distribution Displays overlay of max. 200 distributions
Statistical Data Processing Max. 200 sets of data (also allows overlaying max. 200 data sets)
Time-Series Processing Max. 200 sets of data
3-Dimensional Graphing Max. 200 sets of data
Data Transfer via Clipboard [Image Output]: Outputs entire data sheet or graph only. [Text Output]: Outputs summary data, particle size distribution data, or light intensity distribution data.
Data Sorting Sorts by file name, sample ID, sample number, or refractive index
Output Conditions
Particle Size (μm) Divisions Fixed 51 or 101 divisions : User settable 51 divisions
Particle Amount (%) Divisions Fixed 51 divisions : User settable 51 divisions
Distribution Basis Count, length, area, or volume
Expression of Cumulative Distribution Oversized or undersized
Expression of Frequency Distribution q, q / Δ×, q / Δlog ×
Smoothing Levels 10 levels
Distribution Function Fitting Rosin-Rammler distribution, logarithmic Gaussian distribution
Data Shifting ±10 levels
Report Function Single data sets (6 templates), overlaid data (5 templates), statistical data, time-series data, or 3D data can be selected and output using batch processing
Data Analysis Functions
Scattering Angle Evaluation Function Evaluates scattering characteristics within micro angle regions for samples such as optical films and sheets.
Data Emulation Functions Emulates measurement results from other instruments and measurement principles, using SALD series measurement results.
Mixture Data Simulation Function Simulates particle size distributions using any mixture ratio of multiple particle size distributions.
Data Connection Function Combines two particle size distributions with different measurement ranges at any particle size point to create a single particle size distribution.
Continuous Measurement Function Continuously measures changes in particle size distributions and particle diameters over time, at intervals as short as one second, and saves the results.

Note 5: The LDR method automatically calculates an appropriate refractive index based on consistency between the actual measured light intensity distribution and one reproduced (recalculated) from particle size distribution data. This method was developed by Shimadzu and published in two technical papers. It is sometimes called the "Kinoshita Method", in academic communities, after the name of Shimadzu's engineer.

Top of This Page