50 kN Capstan Grips for Rope

Shimadzu’s 50 kN (11,000 lbf) capstan grips are designed specifically for testing the tensile properties of rope with diameters between 8 and 28 mm (0.31 and 1.1 in). The upper and lower grips incorporate an easy-to-load split-drum and the upper grip has a counterweight attached to align the grips with the loading axis of the test frame.
This grip set includes upper and lower grips with a drum diameter of 180 mm (7.1 in). The grips have alignment grooves on the outside of the split-drum and serrations inside the drum to secure the sample firmly. Standard grip faces are for rope with a diameter of 8 to 12 mm (0.31 to 0.47 in). Additional drum grip faces are available to accommodate ropes with diameters up to 28 mm (1.1 in).
Relevant Materials
Yarn
Relevant Specimens
Rope
Operation
Specimens are inserted between the upper split-drum, wrapped around the upper and lower drums, and fixed between the lower split-drum. The drums self-tighten as the specimens are loaded to ensure that the samples remain secured in place. Adjust the tension of the spring mechanism to alter the initial clamping force and protect samples.
Depress plungers to open the grip faces
Setting of rope
The self-tightening action
Specifications
Maximum Grip Capacity | Applicable Specimen Diameter *1 | Minimum Specimen Length | Temperature Range | Grip Size | Upper Grip Weight | Ø Upper Grip Fitting (Ø pin) |
Ø Lower Grip Fitting (Ø pin)
|
|||
---|---|---|---|---|---|---|---|---|---|---|
Width |
Length
Upper / Lower |
|||||||||
kN | kgf | lbf | mm (in) | mm (in) | °C (°F) | mm (in) | mm (in) | kg (lb) | mm | mm |
50 | 5,000 | 11,000 | 8 to 12 (0.31 to 0.47) |
1800 (70.9) |
-10 to 60 (14 to 140) |
210 (8.3) |
308 / 318 (12.1 / 12.5) |
20 (44) |
35 (13) |
35 (13) |
Note 1: Additional drum grips faces for specimens with diameter of 12 to 16 mm (0.47 to 0.63 in), 16 to 20 mm (0.63 to 0.79 in), 20 to 24 mm (0.79 to 0.94 in), and 24 to 28 mm (0.94 to 1.1 in) are available.
Ordering Information
Part Number | Description |
---|---|
343-07571-04 |
50 kN capstan grips for rope grip set |
Accessories | |
343-08915-01 | Drum grip faces for specimens 8 to 12 mm (0.31 to 0.47 in) in diameter |
343-08915-02 | Drum grip faces for specimens 12 to 16 mm (0.47 to 0.63 in) in diameter |
343-08915-03 | Drum grip faces for specimens 16 to 20 mm (0.63 to 0.79 in) in diameter |
343-08915-04 | Drum grip faces for specimens 20 to 24 mm (0.79 to 0.94 in) in diameter |
343-08915-05 | Drum grip faces for specimens 24 to 28 mm (0.94 to 1.1 in) in diameter |