TW/TX/TXB Series - Specs
Electronic Balances
TXB2201L
| Capacity |
2200g |
|---|---|
| Minimum display |
0.1g |
| Repeatability |
0.1g |
| Linearity |
±0.1g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±15 |
| Pan Size (mm) approx. |
ø160 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TXB4201L
| Capacity |
4200g |
|---|---|
| Minimum display |
0.1g |
| Repeatability |
0.1g |
| Linearity |
±0.2g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±10 |
| Pan Size (mm) approx. |
ø160 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TXB6200L
| Capacity |
6200g |
|---|---|
| Minimum display |
1g |
| Repeatability |
1g |
| Linearity |
±1g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±20 |
| Pan Size (mm) approx. |
ø160 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TXB621L
| Capacity |
620g |
|---|---|
| Minimum display |
0.1g |
| Repeatability |
0.1g |
| Linearity |
±0.1g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±20 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
TXB6201L
| Capacity |
6200g |
|---|---|
| Minimum display |
0.1g |
| Repeatability |
0.1g |
| Linearity |
±0.2g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±5 |
| Pan Size (mm) approx. |
ø160 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TX2202L
| Capacity |
2200g |
|---|---|
| Minimum display |
0.01g |
| Repeatability |
0.01g |
| Linearity |
±0.02g |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
167(W)×181(D) |
| Main Body Dimensions (mm) approx. |
200(W)×291(D)×80(H) |
| Weight (kg) approx. |
2.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TX423L
| Capacity |
420g |
|---|---|
| Minimum display |
0.001g |
| Repeatability |
0.001g |
| Linearity |
±0.002g |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
206(W)×291(D)×241(H) |
| Weight (kg) approx. |
3.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TX3202L
| Capacity |
3200g |
|---|---|
| Minimum display |
0.01g |
| Repeatability |
0.01g |
| Linearity |
±0.02g |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
167(W)×181(D) |
| Main Body Dimensions (mm) approx. |
200(W)×291(D)×80(H) |
| Weight (kg) approx. |
2.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TX323L
| Capacity |
320g |
|---|---|
| Minimum display |
0.001g |
| Repeatability |
0.001g |
| Linearity |
±0.002g |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
206(W)×291(D)×241(H) |
| Weight (kg) approx. |
3.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TXB622L
| Capacity |
620g |
|---|---|
| Minimum display |
0.01g |
| Repeatability |
0.01g |
| Linearity |
±0.02g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±5 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TXB422L
| Capacity |
420g |
|---|---|
| Minimum display |
0.01g |
| Repeatability |
0.01g |
| Linearity |
±0.02g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±10 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TXB222L
| Capacity |
220g |
|---|---|
| Minimum display |
0.01g |
| Repeatability |
0.01g |
| Linearity |
±0.01g |
| Operating Ambient Temperature |
10 - 30 |
| Temperature Coefficient Sensitivity (ppm/C) |
±15 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
199(W)×260(D)×77(H) |
| Weight (kg) approx. |
1.5kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) or 6AA batteries |
| Windows Direct |
● |
TXC623L
| Capacity |
620ct |
|---|---|
| Minimum display |
0.001ct |
| Repeatability |
0.001ct |
| Linearity |
±0.002ct |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
ø80 |
| Main Body Dimensions (mm) approx. |
206(W)×291(D)×241(H) |
| Weight (kg) approx. |
3.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TXC323L
| Capacity |
320ct |
|---|---|
| Minimum display |
0.001ct |
| Repeatability |
0.001ct |
| Linearity |
±0.002ct |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
ø80 |
| Main Body Dimensions (mm) approx. |
206(W)×291(D)×241(H) |
| Weight (kg) approx. |
3.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TX4202L
| Capacity |
4200g |
|---|---|
| Minimum display |
0.01g |
| Repeatability |
0.01g |
| Linearity |
±0.02g |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
167(W)×181(D) |
| Main Body Dimensions (mm) approx. |
200(W)×291(D)×80(H) |
| Weight (kg) approx. |
2.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |
TX223L
| Capacity |
220g |
|---|---|
| Minimum display |
0.001g |
| Repeatability |
0.001g |
| Linearity |
±0.002g |
| Operating Ambient Temperature |
5-40°C |
| Temperature Coefficient Sensitivity (ppm/C) |
±3 |
| Pan Size (mm) approx. |
ø110 |
| Main Body Dimensions (mm) approx. |
206(W)×291(D)×241(H) |
| Weight (kg) approx. |
3.8kg |
| Power requirement |
AC adaptor ( DC12V, 1A ) |