Can I measure linear transmission measurements on integrating spheres?
Relationships Between the Types of Transmission Measurements:
- Subtracting the diffuse transmitted light from the total transmitted light produces the linear transmitted light. However, in actual measurements, the linear transmitted light spreads out before it is detected.
 - Consequently, the linear transmitted light results measured in the standard sample compartment may differ from the linear transmittance calculated as the difference between the total transmitted light and diffuse transmitted light measured using an integrating sphere.