Recent Publications - Composites & Carbon Fiber Reinforced Plastics (CFRP) Testing

Featured Scientific Journals & Papers

Study of resin coating adhesion on GFRP laminate surfaces after UV degradation New!

Jakub Smoleń, Krzysztof Stępień, Anna Mrowiec, Bogusław Mendala, Wiktoria Wilczyńska, Jan Czakiert, Mateusz Kozioł, Study of resin coating adhesion on GFRP laminate surfaces after UV degradation, International Journal of Adhesion and Adhesives, Volume 135, 2024, 103841, ISSN 0143-7496, https://doi.org/10.1016/j.ijadhadh.2024.103841.

Related Products: Universal/Tensile Test Frames

Read/Download

Effect of temperature on high strain-rate damage evolving in CFRP studied by synchrotron-based MHz X-ray phase contrast imaging    New!

Xiyao Sun, David Sory, Kai Liu, Bratislav Lukić, David Simonian, Kwan Lok Wong, Alexander Rack, David Chapman, Nik Petrinic, Daniel Eakins, Effect of temperature on high strain-rate damage evolving in CFRP studied by synchrotron-based MHz X-ray phase contrast imaging, Composites Part B: Engineering, Volume 279, 2024, 111445, ISSN 1359-8368, https://doi.org/10.1016/j.compositesb.2024.111445.

Related Products: High-Speed Video Camera

Read/Download

Experimental Investigation of the Structural Performance of Composite Structures Produced using Additive Manufacturing

Hunter Watts, Ryan Premo, Wayne Huberty, Chris Bounds, & Han-Gyu Kim. (2023). Experimental Investigation of the Structural Performance of Composite Structures Produced using Additive Manufacturing.

Related Products: Universal/Tensile Test Frames

Read/Download

Experimental Characterization of Non-Associative Plasticity Flow Rule Coefficients for the LS-DYNA MAT213 Model

Ryan Premo, Jackob Black, Michael Pereira, Robert K. Goldberg, Trenton M. Ricks, & Han-Gyu Kim. (2023). Experimental Characterization of Non-Associative Plasticity Flow Rule Coefficients for the LS-DYNA MAT213 Model.

Related Products: Universal/Tensile Test Frames

Read/Download

Fabrication of functionalised graphene-PAEK nanocomposites for different manufacturing processes

Yaan Liu, Richard Davies, Paul McCutchion, Adam Chaplin, Stephen Hodge, Elliot Jones, Kayleigh McEwan, Kathryn Hipkins & Oana Ghita (2024) Fabrication of functionalised graphene-PAEK nanocomposites for different manufacturing processes, Virtual and Physical Prototyping, 19:1, e2283884, DOI: 10.1080/17452759.2023.2283884

Related Products: Universal/Tensile Test Frames

Read/Download

Stress Concentration in Open Hole Laminate Composites Under Bending: Potential Application in Dental Implant Prosthesis

Alves, Harlei Augusto Bueno et al. Stress Concentration in Open Hole Laminate Composites Under Bending: Potential Application in Dental Implant Prosthesis. Materials Research [online]. 2022, v. 25 [Accessed 23 November 2021] , e20210235. Available from: . Epub 15 Nov 2021. ISSN 1980-5373. https://doi.org/10.1590/1980-5373-MR-2021-0235.

Related Products: Universal/Tensile Test Frames

Read/Download

Electromechanical properties of carbon-nanostructured elastomeric composites measured by digital image correlation

C. P´erez-Aranda , F. Avil ´es , Electromechanical properties of carbonnanostructured elastomeric composites measured by digital image correlation, Composites Part C: Open Access (2021), doi: https://doi.org/10.1016/j.jcomc.2021.100161

Read/Download

Simple and Reliable Fabrication Method for Polydimethylsiloxane Dielectric Elastomer Actuators Using Carbon Nanotube Powder Electrodes

Ardi Wiranata, Yasuyuki Ishii, Naoki Hosoya, Shingo Maeda Adv. Eng. Mater. 2021, 2001181

Read/Download

Influence of hole quality on fatigue life of drilled CFRP with the different ply orientation angle

Yenigun, B., Kilickap, E. Influence of hole quality on fatigue life of drilled CFRP with the different ply orientation angle. J Braz. Soc. Mech. Sci. Eng. 43, 20 (2021). https://doi.org/10.1007/s40430-020-02719-2

Read/Download

Real-time damage characterization for GFRCs using high-speed synchrotron X-ray phase contrast imaging

Jinling Gao, Nesredin Kedir, Cody D. Kirk, Julio Hernandez, Junyu Wang, Shane Paulson, Xuedong Zhai, Todd Horn, Garam Kim, Jian Gao, Kamel Fezzaa, Francesco De Carlo, Pavel Shevchenko, Tyler N. Tallman, Ronald Sterkenburg, Giuseppe R. Palmese, Weinong Chen, Real-time damage characterization for GFRCs using high-speed synchrotron X-ray phase contrast imaging, Composites Part B: Engineering, Volume 207,
2021, 108565, ISSN 1359-8368, https://doi.org/10.1016/j.compositesb.2020.108565.

Read/Download

Enhancing the Ductility of a Reinforced Concrete Beam using Engineered Cementitious Composite

M A Bastian et al 2020 IOP Conf. Ser.: Earth Environ. Sci. 506 012044

Read/Download

Cyclic strength of polyester acrylate composites

Vladimir Erofeev et al 2020 IOP Conf. Ser.: Mater. Sci. Eng. 896 012110

Read/Download

Mode-I behavior of adhesively bonded composite joints at high loading rates

Suraj Ravindran, Subramani Sockalingam, Karan Kodagali, Addis Kidane, Michael A. Sutton, Brian Justusson, Jenna Pang, Mode-I behavior of adhesively bonded composite joints at high loading rates, Composites Science and Technology, Volume 198, 2020, 108310

Read/Download

Electrodeposition of Ag/CNT Composite Films from Iodide Plating Baths

Susumu Arai et al 2020 J. Electrochem. Soc. 167 122515

Read/Download

Transparent Nacre‐like Composites Toughened through Mineral Bridges

Advanced Functional Materials
Tommaso Magrini, Simon Moser, Madeleine Fellner, Alessandro Lauria, Florian Bouville, André R. Studart

Read/Download

Evaluation of the stiffening mechanism based on micro-sized particle inclusions in laminated composites

Mat. Res. vol.22 no.4 São Carlos 2019 Epub Oct 17, 2019

Read/Download

Effect of fiber amount on mechanical and thermal properties of (3-aminopropyl) triethoxysilane treated basalt fiber reinforced ABS composites

Materials Research Express, Volume 6, Number 11

Read/Download

News / Events

Learn more