Pass/Fail Judgment of Automotive Window Tint Film Using the Spectral Evaluation Function of LabSolutions UV-Vis Software

In this article we performed measurement of automotive window tint film using the spectral evaluation function of LabSolutions UV-Vis software. This example demonstrates the effectiveness of using the spectral evaluation function of LabSolutions UV-Vis software to make a pass/fail judgment easily. The use of this function reduces the effort required to obtain pass/fail judgments from measurements and enables various quality inspections with great efficiency.