Determination of Volatile Organic Compounds in Water-based Paints and Varnishes Using GC-MS

A general GC-MS method was developed, using the Shimadzu GCMS-QP2010 Ultra, for determination of 35 VOCs commonly found in water-based paints and varnishes. A wide range of calibration was established with good correlative coefficient, as well as good repeatability. The results even demonstrated the capability of using this instrument for the determination of compounds which were not calibrated, in preparation to fulfil the requirements of any possible future regulations.