FTIR Plastic Analyzer Method Package - Specs
Fourier Transform Infrared Spectrophotometer Plastic Analysis System
Target Sample Size and Search Method
| Item | Specifications |
|---|---|
| Sample Size | Plastic approximately 0.3 mm or larger There is no function to measure the size or quantity of the plastic. An infrared microscope is effective for analyzing plastic samples less than 0.3 mm in size. |
| Search Method | Search matching using a special library There is no function to determine the degree of deterioration. This library contains infrared spectra differing with respect to the UV irradiation time, heating time, and heating temperature. However, the irradiation and heating conditions noted in the data matches from library searches of the analyzed samples measured are at best reference values. Be aware that they do not indicate that the sample was placed under identical conditions. |