HMV-G Series - Specs
Micro Vickers Hardness Testers
HMV-G31ST
Monochrome Camera with Electric Turret
HMV-G31 Series
| Model P/N |
344-04277-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G Series
| Test force rang |
0.0098 to 19.6 N |
|---|---|
| Reading method |
Automatic (G31) Manual (G30) |
| Maximum number of indenters and object lenses installed |
S: Indenters 1, Object lenses 2 |
| With electrically driven revolver |
HMV-G31ST/G31DT |
HMV-G31-XY-D-HC
Color Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04294-□□ |
|---|---|
| Autofocus Function |
N |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-XY-S-HC
Color Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04293-□□ |
|---|---|
| Autofocus Function |
N |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-FA-D-HC
Color Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04292-□□ |
|---|---|
| Autofocus Function |
Y |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× (Super-long |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-FA-S-HC
Color Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04291-□□ |
|---|---|
| Autofocus Function |
Y |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× (Super-longWorking Distanse) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-XY-D
Monochrome Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04282-□□ |
|---|---|
| Autofocus Function |
N |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-XY-S
Monochrome Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04281-□□ |
|---|---|
| Autofocus Function |
N |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-FA-D
Monochrome Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04280-□□ |
|---|---|
| Autofocus Function |
Y |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× (Super-long |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G31-FA-S
Monochrome Camera with Electric Turret
HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)
| Model P/N |
344-04279-□□ |
|---|---|
| Autofocus Function |
Y |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 50 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3 |
| Image Acquisition Functions |
Total image acquisition function and edge detection function |
| Pattern Settings Items |
Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division, |
| XY Stage |
Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm |
| Test Force |
16 stages in total |
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 µm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, |
| Standard Objective Lenses Provided |
40× (Super-longWorking Distanse) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows®10 (64 bit edition) |
*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.
HMV-G30DT
Monochrome Camera with Electric Turret
HMV-G30 Series
| Model P/N |
344-04276-□□ |
|---|---|
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Thermal printer |
| External Output : USB |
Transfer of test results to a USB flash drive (CSV format) |
| Results Displayed : Graphical Display |
Variance graph, histogram, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| Effective Measurement Range (For 40× objective lens) |
250×250μm |
| Test Force |
16 stages in total |
| Eyepiece |
×10 |
| Indentation Reading System |
Manual readings via an optical microscope |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2× (1 empty) |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31S-HC
Color Camera without Electric Turret
HMV-G31 Series
| Model P/N |
344-04287-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G30D
Monochrome Camera without Electric Turret
HMV-G30 Series
| Model P/N |
344-04272-□□ |
|---|---|
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Thermal printer |
| External Output : USB |
Transfer of test results to a USB flash drive (CSV format) |
| Results Displayed : Graphical Display |
Variance graph, histogram, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| Effective Measurement Range (For 40× objective lens) |
250×250μm |
| Test Force |
16 stages in total |
| Eyepiece |
×10 |
| Indentation Reading System |
Manual readings via an optical microscope |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2× (1 empty) |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G30ST
Monochrome Camera with Electric Turret
HMV-G30 Series
| Model P/N |
344-04275-□□ |
|---|---|
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Thermal printer |
| External Output : USB |
Transfer of test results to a USB flash drive (CSV format) |
| Results Displayed : Graphical Display |
Variance graph, histogram, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| Effective Measurement Range (For 40× objective lens) |
250×250μm |
| Test Force |
16 stages in total |
| Eyepiece |
×10 |
| Indentation Reading System |
Manual readings via an optical microscope |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G30S
Monochrome Camera without Electric Turret
HMV-G30 Series
| Model P/N |
344-04271-□□ |
|---|---|
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Thermal printer |
| External Output : USB |
Transfer of test results to a USB flash drive (CSV format) |
| Results Displayed : Graphical Display |
Variance graph, histogram, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| Effective Measurement Range (For 40× objective lens) |
250×250μm |
| Test Force |
16 stages in total |
| Eyepiece |
×10 |
| Indentation Reading System |
Manual readings via an optical microscope |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31DT-HC
Color Camera with Electric Turret
HMV-G31 Series
| Model P/N |
344-04290-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2× (1 empty) |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31D-HC
Color Camera without Electric Turret
HMV-G31 Series
| Model P/N |
344-04288-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2× (1 empty) |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31DT
Monochrome Camera with Electric Turret
HMV-G31 Series
| Model P/N |
344-04278-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2× (1 empty) |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31D
Monochrome Camera without Electric Turret
HMV-G31 Series
| Model P/N |
344-04274-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× 10× (2 empty) |
| Maximum Number of Objective Lens Attachments |
4 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
2× (1 empty) |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31ST-HC
Color Camera with Electric Turret
HMV-G31 Series
| P/N |
344-04289-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually
HMV-G31S
Monochrome Camera without Electric Turret
HMV-G31 Series
| Model P/N |
344-04273-□□ |
|---|---|
| Effective Measurement Range (For 40× objective lens) |
Monochrome Camera: 120 × 90 μm |
| Power supply |
Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz) |
| Weight |
Approx. 45 kg |
| External Dimensions |
Approx. W350 × D570 × H540 mm |
| External Output : Printer |
Printer output from a PC via software |
| Results Displayed : Graphical Display |
Variance graph, depth of hardening graph*6 |
| Results Displayed : Displayed Items |
Data No., diagonal line length, hardness, conversion value, average, standard deviation, |
| Data Processing Functions |
① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3 |
| XY Stage |
Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm |
| Digital Camera : Color |
USB Connection (USB 3.0 Super Speed) |
| Test Force |
16 stages in total |
| Digital Camera : Monochrome |
USB Connection (USB 2.0) |
| Indentation Reading System |
Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window |
| Standard Objective Lenses Provided |
40× (1 empty) |
| Maximum Number of Objective Lens Attachments |
2 |
| Standard Indenter Provided |
Vickers Indenter |
| Maximum Number of Indenter Attachments |
1 |
| Test Force Duration Time |
User-designated settings from 0 to 999 sec*2, in 1 sec increments |
| Loading Unit |
Automatic loading and automatic force changing |
| PC Provided*8 |
OS: Windows® 10 (64 bit edition) |
*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually