Tensile Test Methods for Plastics: ISO 527 and JIS K 7161 - Specs
1B Specimens
ISO 527 and JIS K 7161 require a test force accuracy that meets ISO 7500-1 Class 1 and JIS B 7721 Class 1, accuracy within 1% of the indicated test force.Shimadzu’s AG-X plus series, AGS-X series, and EZ-X series test frames and load cells meet the test force accuracy requirements of ISO 527 and JIS K 7161.
Test force accuracy of ±1%
| Full length, l3 |
150 |
|---|---|
| Parallel length, l1 |
60 |
| Gauge length, L0 |
50 |
| Parallel section width, b1 |
10 |
| Thickness, h |
4 |
| Grip section width, b2 |
20 |
| Grip face length, L |
115 |
1A Specimens
ISO 527 and JIS K 7161 require a test force accuracy that meets ISO 7500-1 Class 1 and JIS B 7721 Class 1, accuracy within 1% of the indicated test force.Shimadzu’s AG-X plus series, AGS-X series, and EZ-X series test frames and load cells meet the test force accuracy requirements of ISO 527 and JIS K 7161.
Test force accuracy of ±1%
| Full length, l3 |
170 |
|---|---|
| Parallel length, l1 |
80 |
| Gauge length, L0 |
75,50 |
| Parallel section width, b1 |
10 |
| Thickness, h |
4 |
| Grip section width, b2 |
20 |
| Grip face length, L |
115 |