AUTOGRAPH AGS-X2 Series Precision Universal Testing Machines - Specs
Precision Universal Testing Machines
| Model | AGS-20kNX2D | AGS-50kNX2D | AGS-100kNX2 | AGS-300kNX2 | ||
|---|---|---|---|---|---|---|
![]() |
![]() |
![]() |
![]() |
|||
| Table-top Type | Floor Type | |||||
| Force Measurement |
Accuracy | High-Precision Type (1/500, ±0.5%) |
Within ±0.5% indicated test force (at 1/500 to 1/1 load cell rating) | Within ±0.5% indicated test force (at 1/250 to 1/1 load cell rating) | ||
| Conforms to EN 10002-2 Grade 0.5, ISO 7500-1 Class 0.5, BS 1610 Class 0.5, ASTM E4, and JIS B7721 Class 0.5.*1 | ||||||
| Standard-Precision Type (1/500, ±1%) |
Within ±1% indicated test force (at 1/500 to 1/1 load cell rating) | |||||
| Conforms to EN 10002-2 Grade 1, ISO 7500-1 Class 1, BS 1610 Class 1, ASTM E4, and JIS B7721 Class 1.*1 | ||||||
| Calibration | Automatic test force calibration: select tensile, compression, or tensile and compression | |||||
| Crosshead | Speed Range | 0.001 to 2000 mm/min (stepless) | 0.0001 to 1000 mm/min (stepless) | 0.0001 to 500 mm/min (stepless) | ||
| Max. Return Speed | 2200 mm/min | 1100 mm/min | 550 mm/min | |||
| Crosshead Speed Accuracy*2 | ±0.1% | |||||
| Crosshead Speed and Permitted Test Force | To load cell capacity across entire speed range | 0.001–200 kN: 0.001–500 mm/min (entire speed range) 200–300 kN: 0.001–400 mm/min |
||||
| Crosshead – Table Distance (Tensile stroke) *3 | 1250 mm (765 mm, MWG) | 1210 mm (745 mm, MWG) | 1255 mm (745 mm, MWG) | 1475 mm (635 mm, MWG) | ||
| Effective Test Width | 425 mm | 600 mm | ||||
| Crosshead Position Detection | Measurement Method | Optical encoder | ||||
| Display Method | Digital display (display resolution: 0.001 mm) | |||||
| Positional Accuracy | ±0.1% indicated value or ±0.01 mm, whichever is larger | |||||
| Data Capture Rate | 1000 Hz max.*4 | |||||
| Test Method Files | 40 files (PC link: 20 files, standalone controller: 20 files) | |||||
| Standard Functions |
|
|||||
| Accessories | Load Cell (with CAL cable), Power cable (5 m), turning rod, cable clamps, instruction manual | |||||
| Dimensions | ![]() |
![]() |
||||
| W718 × D641 × H1633 mm | W945 × D725 × H2164 mm | W945 × D725 × H2414 mm | ||||
| Weight | 235 kg | 260 kg | 525 kg | 675 kg | ||
| Power Requirements | Single phase AC 200–230 50/60 Hz 4.0 kVA | 400 V model: Three phases AC 380–440 V 50/60 Hz 4.5 kVA 200 V model: Three phases AC 200–230 V 50/60 Hz 6.5 kVA |
400 V model: Three phases AC 380–440 V 50/60 Hz 5.5 kVA 200 V model: Three phases AC 200–230 V 50/60 Hz 7.5 kVA |
|||
| Supply voltage fluctuations within ±10% of the set value. D-class (100 Ω max.) grounding resistance. |
Supply voltage fluctuations within ±10% of the set value. 400 V model: C-class (10 Ω max.) grounding resistance. 200 V model: D-class (100 Ω max.) grounding resistance. |
|||||
| Operating Environment | Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation) Floor vibrations: frequency 10 Hz max., amplitude 5 μm max. |
|||||
- Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, ASTM E4 standards, and JIS B7721.
- Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
- The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
- TRAPEZIUM X-V is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain
control (auto tuning) are used, the sampling speed becomes 10 msec. - Dataletty (option) and TRAPEZIUM X-V can not be used together.