Compression Test Jig for Foam Specimens
Features:
- Applicable to compression testing rubber foam and urethane foam specimens
- Compliant with ASTM D3574 and JIS K6384 standards
- Perforated support plate enables air to escape from the foam during testing
- For testing below 1 kN (220 lbf)
Relevant Materials:
Rubber Foam, Urethane Foam
Relevant Specimens:
Cuboids
Relevant Standards:
ASTM D3574, JIS K6384
This compression test jig is specifically designed to test rubber foam and urethane foam specimens that are molded, cored from a larger sheet, or shaped, for example, having a dimpled pattern.
The compression test jig for foam specimens consists of a 200 mm (7.9 in) diameter upper compression plate and a larger 400 mm (15.7 in) by 400 mm lower support plate. The lower plate contains holes 6.5 mm (0.26 in) in diameter, spaced 20 mm (0.79 in) apart. The perforations are designed to allow air to escape from the foam during testing.
Common tests applicable to rubber foam and urethane foam include compression to a specified deflection or force, where the resulting force or deflection, respectively, are measured, and maintenance of a constant deflection with measurement of recovery.
Compression test kits for foam specimens are available in certain regions. In addition to the compression test jig, these kits include a compression and bending loading jig. Please contact your local Shimadzu representative for details.
This compression test jig for foam specimens cannot be installed on universal testers with safety covers attached.
News / Events
-
SAMPE 2026 (Society for the Advancement of Material and Process Engineering)
April 28-29
Seattle Convention Center
Seattle, WA
Booth #N7
-
Medical Design & Manufacturing West 2026
February 3-5
Anaheim Convention Center
Anaheim, CA
Booth #2283 -
Shimadzu Scientific Instruments Launches New AUTOGRAPH AGS-V Series
Shimadzu Scientific Instruments (SSI) introduces the AUTOGRAPH AGS-V Series Tabletop Precision Universal Testing Machines. Featuring a wide selection of load cell capacities, versatile control options and compatible accessories, the AGS-V Series delivers dependable testing of diverse material types.