In-Plane Compression Test Jigs for Composite Materials
Features:
- Specially designed for testing the in-plane strength properties of thin, rigid plastics and composite materials
- Maximum capacity of 5 kN (1,100 lbf)
- Available as an ASTM D695 and ASTM D3846 compliant jig or a JIS K7076 (method A) and JIS K7018 (method 1) compliant jig
- Compressive force is applied to the end surface of the specimen
Relevant Materials:
Plastics, Composites
Relevant Standards:
ASTM D695, ASTM D3846, JIS K7018 (Method 1), JIS K7076 (Method A)
In-plane compression test jigs for composite materials are specially designed for testing the in-plane strength properties of thin, rigid plastics, both non-reinforced and reinforced, and other composite materials. Specimens are held in the jigs in a vertical direction and a compressive force is applied to the specimen’s end surface.
Two in-plane compression test jigs for composite materials are available: an ASTM D695 and ASTM D3846 compliant jig and a JIS K7076 (method A) and JIS K7018 (method 1) compliant jig. A 100 mm (3.9 in) diameter spherically seated compression plate set is used to apply the compressive force and should be ordered along with the jigs.
In certain regions, kits are available comprising one type of in-plane compression test jig for composite materials, a 100 mm diameter spherically seated compression plate set, and a compression and bending loading jig matched to a specific model universal tester. Please consult with your local Shimadzu representative for further information.
Additional items needed for operation:
- 100 mm diameter spherically seated compression plate set
News / Events
-
SAMPE 2026 (Society for the Advancement of Material and Process Engineering)
April 28-29
Seattle Convention Center
Seattle, WA
Booth #N7
-
Medical Design & Manufacturing West 2026
February 3-5
Anaheim Convention Center
Anaheim, CA
Booth #2283 -
Shimadzu Scientific Instruments Launches New AUTOGRAPH AGS-V Series
Shimadzu Scientific Instruments (SSI) introduces the AUTOGRAPH AGS-V Series Tabletop Precision Universal Testing Machines. Featuring a wide selection of load cell capacities, versatile control options and compatible accessories, the AGS-V Series delivers dependable testing of diverse material types.