UW420H

UW (with built-in calibration weights)

Capacity

420

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.002

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX420H

UW (with built-in calibration weights)

Capacity

420 g

Minimum display

0.001g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW1020H

UW (with built-in calibration weights)

Capacity

1,020 g

Minimum display

0.001g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW2200H

UW (with built-in calibration weights)

Capacity

2,200 g

Minimum display

0.01g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW4200H

UW (with built-in calibration weights)

Capacity

4,200 g

Minimum display

0.01g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW6200H

UW (with built-in calibration weights)

Capacity

6,200 g

Minimum display

0.01g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW420S

UW (with built-in calibration weights)

Capacity

420 g

Minimum display

0.01g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW820S

UW (with built-in calibration weights)

Capacity

820 g

Minimum display

0.01g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW4200S

UW (with built-in calibration weights)

Capacity

4,200 g

Minimum display

0.1g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW8200S

UW (with built-in calibration weights)

Capacity

8,200 g

Minimum display

0.1g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX220H

UW (with built-in calibration weights)

Capacity

220 g

Minimum display

0.001g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX620H

UW (with built-in calibration weights)

Capacity

620 g

Minimum display

0.001g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW620H

UW (with built-in calibration weights)

Capacity

620 g

Minimum display

0.001g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX820H

UW (with built-in calibration weights)

Capacity

820 g

Minimum display

0.001g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX1020H

UW (with built-in calibration weights)

Capacity

1,020 g

Minimum display

0.001g

Windows Direct

●

UX2200H

UW (with built-in calibration weights)

Capacity

2,200 g

Minimum display

0.01g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX4200H

UW (with built-in calibration weights)

Capacity

4,200 g

Minimum display

0.01g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX6200H

UW (with built-in calibration weights)

Capacity

6,200 g

Minimum display

0.01g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX420S

UW (with built-in calibration weights)

Capacity

420 g

Minimum display

0.01g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX820S

UW (with built-in calibration weights)

Capacity

820 g

Minimum display

0.01g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX4200S

UW (with built-in calibration weights)

Capacity

4,200 g

Minimum display

0.1g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX8200S

UW (with built-in calibration weights)

Capacity

8,200 g

Minimum display

0.1g

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW820H

UW (with built-in calibration weights)

Capacity

820 g

Minimum display

0.001g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW420H

UW (with built-in calibration weights)

Capacity

420 g

Minimum display

0.001g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UW620H

UW (with built-in calibration weights)

Capacity

620

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.002

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX220H

UX (Standard model)

Capacity

220

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.002

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UW820H

UW (with built-in calibration weights)

Capacity

820

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.003

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UW1020H

UW (with built-in calibration weights)

Capacity

1020

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.003

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UW2200H

UW (with built-in calibration weights)

Capacity

2200

Minimum display

0.01

Repeatability

≤0.01

Linearity

±0.02

Response Time

1.5–2.5

Pan Size (mm) approx

170 × 180

Read more
Show Less

UW4200H

UW (with built-in calibration weights)

Capacity

4200

Minimum display

0.01

Repeatability

≤0.01

Linearity

±0.02

Response Time

1.5–2.5

Pan Size (mm) approx

170 × 180

Read more
Show Less

UW6200H

UW (with built-in calibration weights)

Capacity

6200

Minimum display

0.01

Repeatability

≤0.01

Linearity

±0.02

Response Time

1.5–2.5

Pan Size (mm) approx

170 × 180

Read more
Show Less

UW420S

UW (with built-in calibration weights)

Capacity

420

Minimum display

0.01

Repeatability

≤0.008

Linearity

±0.01

Response Time

0.7–1.2

Pan Size (mm) approx

108 × 105

Read more
Show Less

UW820S

UW (with built-in calibration weights)

Capacity

820

Minimum display

0.01

Repeatability

≤0.008

Linearity

±0.01

Response Time

0.7–1.2

Pan Size (mm) approx

108 × 105

Read more
Show Less

UW4200S

UW (with built-in calibration weights)

Capacity

4200

Minimum display

0.1

Repeatability

≤0.08

Linearity

±0.1

Response Time

0.7–1.2

Pan Size (mm) approx

170 × 180

Read more
Show Less

UW8200S

UW (with built-in calibration weights)

Capacity

8200

Minimum display

0.1

Repeatability

≤0.08

Linearity

±0.1

Response Time

0.7–1.2

Pan Size (mm) approx

170 × 180

Read more
Show Less

UX420H

UX (Standard model)

Capacity

420

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.002

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UW220H

UW (with built-in calibration weights)

Capacity

220 g

Minimum display

0.001g

PSC

●

ClockCAL

●

GLP/GMP/ISO calibration report

●

Windows Direct

●

Read more
Show Less

UX620H

UX (Standard model)

Capacity

620

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.002

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX820H

UX (Standard model)

Capacity

820

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.003

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX1020H

UX (Standard model)

Capacity

1020

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.003

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX2200H

UX (Standard model)

Capacity

2200

Minimum display

0.01

Repeatability

≤0.01

Linearity

±0.02

Response Time

1.5–2.5

Pan Size (mm) approx

170 × 180

Read more
Show Less

UX4200H

UX (Standard model)

Capacity

4200

Minimum display

0.01

Repeatability

≤0.01

Linearity

±0.02

Response Time

1.5–2.5

Pan Size (mm) approx

170 × 180

Read more
Show Less

UX6200H

UX (Standard model)

Capacity

6200

Minimum display

0.01

Repeatability

≤0.01

Linearity

±0.02

Response Time

1.5–2.5

Pan Size (mm) approx

170 × 180

Read more
Show Less

UX420S

UX (Standard model)

Capacity

420

Minimum display

0.01

Repeatability

≤0.008

Linearity

±0.01

Response Time

0.7–1.2

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX820S

UX (Standard model)

Capacity

820

Minimum display

0.01

Repeatability

≤0.008

Linearity

±0.01

Response Time

0.7–1.2

Pan Size (mm) approx

108 × 105

Read more
Show Less

UX4200S

UX (Standard model)

Capacity

4200

Minimum display

0.1

Repeatability

≤0.08

Linearity

±0.1

Response Time

0.7–1.2

Pan Size (mm) approx

170 × 180

Read more
Show Less

UX8200S

UX (Standard model)

Capacity

8200

Minimum display

0.1

Repeatability

≤0.08

Linearity

±0.1

Response Time

0.7–1.2

Pan Size (mm) approx

170 × 180

Read more
Show Less

UW220H

UW (with built-in calibration weights)

Capacity

220

Minimum display

0.001

Repeatability

≤0.001

Linearity

±0.002

Response Time

1.5–2.5

Pan Size (mm) approx

108 × 105

Read more
Show Less
{"title":"Specification Sheet Downloads","description":"Download the latest specification sheets.","source":"product","key":3529,"max":30,"filter_types":["spec_sheet"],"link_title":"View other Downloads","link_url":""} {"title":"Downloads","description":"Download the latest brochure.","source":"product","key":3529,"max":30,"filter_types":["brochures"],"link_title":"View other Downloads","link_url":"","pdf_links":[]}