Enhance Material Testing Efficiency with USF-2000A: Explore Now! - Specs
Ultrasonic Fatigue Testing System
USF-2000A
| Test frequency |
20 kHz ±500 Hz (recommended test range: 20 kHz ±30 Hz) |
|---|---|
| Vibration at horn tip |
±10 to ±50 μm |
| Test stress range |
Stress given ±10 to ±50 μm displacement of sample |
| Stress ratio |
-1 |
| Testable materials |
Materials that can be resonated at 20 kHz and generate minimal heat during resonance |
| Not-testable materials |
- Materials that cannot resonate at 20 kHz |
| Power Requirements |
3-phase 200 V: 2 kVA (air compressor) , 1-phase 200V: 3.5 kVA (ultrasonic fatigue testing system) , 1-phase 100V: 1 kVA (computer, displacement logger, air dryer, etc.) |
| Standard contents |
USF-2000A Ultrasonic Fatigue Testing System main unit (including table), ultrasonic resonance system, control computer,ultrasonic testing control and measurement software, and cooling unit (air dryer and compressed air lines) |
| Required optional products |
Air compressor (for regions with 50 Hz or 60 Hz power) 3-phase 200 V: 2 kVA |
Note: Systems can be selected without an air compressor in cases where the customer will supply the compressed air. A 150 L/m flow rate of compressed air at a minimum 0.2 MPa is required.
USF-2000A
| Test frequency |
20 kHz ± 500 Hz |
|---|---|
| Test stress |
180 to 900 MPa (in the case of a steel circular taper specimen) |
| Stress ratio |
-1 |