Recent Publications - High-Speed Video Camera

Featured Scientific Journals & Papers

Effect of temperature on high strain-rate damage evolving in CFRP studied by synchrotron-based MHz X-ray phase contrast imaging    New!

Xiyao Sun, David Sory, Kai Liu, Bratislav Lukić, David Simonian, Kwan Lok Wong, Alexander Rack, David Chapman, Nik Petrinic, Daniel Eakins, Effect of temperature on high strain-rate damage evolving in CFRP studied by synchrotron-based MHz X-ray phase contrast imaging, Composites Part B: Engineering, Volume 279, 2024, 111445, ISSN 1359-8368, https://doi.org/10.1016/j.compositesb.2024.111445.

Related Industries: High Speed Mechanical Testing and Imaging, Composites & Carbon Fiber Reinforced Plastics (CFRP) Testing

Read/Download

 

An Acoustic Device for Ultra High-Speed Quantification of Cell Strain During Cell–Microbubble Interaction

Pattinson, O., Keller, S., Evans, N., Pierron, F., & Carugo, D. (0). An Acoustic Device for Ultra High-Speed Quantification of Cell Strain During Cell–Microbubble Interaction. ACS Biomaterials Science & Engineering.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Visualization of end-gas auto-ignition during PREMIER combustion in a dual-fuel gas engine

Nobuyuki Kawahara, Eiji Tomita, Visualization of end-gas auto-ignition during PREMIER combustion in a dual-fuel gas engine, The Proceedings of the International symposium on diagnostics and modeling of combustion in internal combustion engines, 2022, Volume 2022.10, Session ID C9-3, Pages C9-3-, Released on J-STAGE January 25, 2023, Online ISSN 2424-2918, https://doi.org/10.1299/jmsesdm.2022.10.C9-3, https://www.jstage.jst.go.jp/article/jmsesdm/2022.10/0/2022.10_C9-3/_article/-char/en

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Characterization of local mechanical properties of Al/Cu Magnetic Pulse Welded joints under high strain rates using synchrotron X-ray imaging

Benjamin Zielinski, Tarik Sadat, Bratislav Lukić, Grégory Haugou, Hervé Morvan, Alexander Rack, Eric Markiewicz, Laurent Dubar, Characterization of local mechanical properties of Al/Cu Magnetic Pulse Welded joints under high strain rates using synchrotron X-ray imaging, Materials Letters, Volume 337, 2023, 133943, ISSN 0167-577X, https://doi.org/10.1016/j.matlet.2023.133943. (https://www.sciencedirect.com/science/article/pii/S0167577X23001283)

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Mesoscale shock structure in particulate composites

Ravindran, S., Gandhi, V., Lawlor, B., & Ravichandran, G.. (2022). Mesoscale shock structure in particulate composites.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

A Comparison of High-Rate Tensile Failure Methods for Structural Adhesives

Breedlove, E.L., Powers, R., Kennedy, M., Al Tameemi, M., Priester, J. (2023). A Comparison of High-Rate Tensile Failure Methods for Structural Adhesives. In: Mates, S., Eliasson, V., Allison, P. (eds) Dynamic Behavior of Materials, Volume 1. SEM 2022. Conference Proceedings of the Society for Experimental Mechanics Series. Springer, Cham. https://doi.org/10.1007/978-3-031-17453-7_17

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Quantifying Thermal Output of Energetic Materials: LDRD Final Report

Kearney, Sean, Swain, William, Stacy, Shawn, Halls, Benjamin, wwerik,, Marinis, Ryan, Richardson, Daniel, Marsh, Andrew, and Mazumdar, Yi. Quantifying Thermal Output of Energetic Materials: LDRD Final Report.. United States: N. p., 2022. Web. doi:10.2172/1892464.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Nano-additive manufacturing of multilevel strengthened aluminum matrix composites

Chenwei Shao, Haoyang Li, Yankun Zhu, Peng Li, Haoyang Yu, Zhefeng Zhang3Herbert Gleiter, André McDonald and James Hogan Accepted Manuscript online 19 October 2022 © 2022 The Author(s). Published by IOP Publishing Ltd on behalf of the IMMT

Related Industries: High Speed Mechanical Testing and Imaging, Additive Manufacturing

Read/Download

 

The Novel "Fracture" Gun at the DEVCOM Army Research Laboratory for Precise, Highly Instrumented Impact Experiments

Meredith, Christopher. (2022). The Novel "Fracture" Gun at the DEVCOM Army Research Laboratory for Precise, Highly Instrumented Impact Experiments.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

High-Speed Imaging Diagnostics of Hypervelocity Projectile-Water Droplet Interactions

G. D. Lukasik, J. A. Rogers, T. E. Lacy, and W. D. Kulatilaka, "High-Speed Imaging Diagnostics of Hypervelocity Projectile-Water Droplet Interactions," in Optical Sensors and Sensing Congress 2022 (AIS, LACSEA, Sensors, ES), Technical Digest Series (Optica Publishing Group, 2022), paper LTu5B.5.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

An explicit phase field method for dynamic fracture

Huilong Rena , Xiaoying Zhuanga , Cosmin Anitescub , Timon Rabczuk - ICILSM 2022

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Damage accumulation mechanisms during dynamic compressive failure of boron carbide

Brendan M.L. Koch, Haoyang Li, Calvin Lo, Jonathan Ligda, James David Hogan, Damage accumulation mechanisms during dynamic compressive failure of boron carbide, Journal of the European Ceramic Society, 2022, , ISSN 0955-2219, https://doi.org/10.1016/j.jeurceramsoc.2022.05.052. (https://www.sciencedirect.com/science/article/pii/S0955221922004101)

Related Industries: High Speed Mechanical Testing and Imaging

Spatial evolution of nitric oxide in ns-discharges using a 250 kHz optical parametric oscillator

Boris S. Leonov, Anuj Rekhy, Yue Wu, James R. Creel, and Christopher M. Limbach, "Spatial evolution of nitric oxide in ns-discharges using a 250 kHz optical parametric oscillator," Opt. Continuum 1, 1278-1285 (2022)

Related Industries: High Speed Mechanical Testing and Imaging

3D optical diagnostics for explosively driven deformation and fragmentation

Daniel R. Guildenbecher, Elizabeth M.C. Jones, Elise M. Hall, Phillip L. Reu, Timothy J. Miller, Francisco Perez, Andrew D. Thompson, James Patrick Ball, 3D optical diagnostics for explosively driven deformation and fragmentation, International Journal of Impact Engineering, Volume 162, 2022, 104142, ISSN 0734-743X, https://doi.org/10.1016/j.ijimpeng.2021.104142.

Related Industries: High Speed Mechanical Testing and Imaging

Supersonic jet by blast wave focusing

N. Apazidis, S. Sembian, and M. Liverts , "Supersonic jet by blast wave focusing", Physics of Fluids 33, 126101 (2021) https://doi.org/10.1063/5.0068309

Related Industries: High Speed Mechanical Testing and Imaging

Hypervelocity impact response of monolithic UHMWPE and HDPE plates

Jacob A. Rogers, Aniket Mote, Paul T. Mead, Khari Harrison, Gavin D. Lukasik, Kalyan Raj Kota, Waruna D. Kulatilaka, Justin W. Wilkerson, Thomas E. Lacy, Hypervelocity impact response of monolithic UHMWPE and HDPE plates, International Journal of Impact Engineering, Volume 161, 2022, 104081, ISSN 0734-743X, https://doi.org/10.1016/j.ijimpeng.2021.104081.

Related Industries: High Speed Mechanical Testing and Imaging

Density, strain rate and strain effects on mechanical property evolution in polymeric foams

Kapil Bharadwaj Bhagavathula, Christopher S Meredith, Simon Ouellet, Dan L Romanyk, James David Hogan, Density, strain rate and strain effects on mechanical property evolution in polymeric foams, International Journal of Impact Engineering, Volume 161, 2022, 104100, ISSN 0734-743X, https://doi.org/10.1016/j.ijimpeng.2021.104100.

Related Industries: High Speed Mechanical Testing and Imaging

Diminishing comminution of urinary stones with subsequent laser pulses

Yuri A. Pishchalnikov Applaud Medical, Inc., 953 Indiana St., San Francisco, CA 94107, yuri.pishchalnikov@applaudmedical.com William M. Behnke-Parks Applaud Medical, Inc., San Francisco, CA Marshall L. Stoller Dept. of Urology, Univ. of California San Francisco, San Francisco, CA, "Diminishing comminution of urinary stones with subsequent laser pulses", The Journal of the Acoustical Society of America 150, A329-A329 (2021) https://doi.org/10.1121/10.0008467

Related Industries: High Speed Mechanical Testing and Imaging

Strain-Rate-Dependent mechanical behavior of a non-Equimolar CoCrFeMnNi high entropy alloy with a segmented coarse grain structure

Haoyang Li, Chenwei Shao, Okan K. Orhan, David Funes Rojas, Mauricio Ponga, James D. Hogan, Strain-Rate-Dependent mechanical behavior of a non-Equimolar CoCrFeMnNi high entropy alloy with a segmented coarse grain structure, Materialia, Volume 21, 2022, 101271, ISSN 2589-1529, https://doi.org/10.1016/j.mtla.2021.101271. (https://www.sciencedirect.com/science/article/pii/S258915292100274X)

Related Industries: High Speed Mechanical Testing and Imaging

AIAA SciTech Forum and Exposition 2023 Papers

Time-Resolved Stagnation Pressure Measurement Technique in a Rotating Detonation Rocket Combustor

Kevin Dille, Mark Frederick, Carson D. Slabaugh and Stephen D. Heister. "Time-Resolved Stagnation Pressure Measurement Technique in a Rotating Detonation Rocket Combustor," AIAA 2023-1871. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Digital Holography for Investigating Front-Edge Instabilities of Liquid Jets in Supersonic Crossflows

Joshua A. Johnson, Suresh Menon and Yi C. Mazumdar. "Digital Holography for Investigating Front-Edge Instabilities of Liquid Jets in Supersonic Crossflows," AIAA 2023-0804. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Time resolved visualization of liquid jet interaction with H2-air Rotating Detonations using MHz-rate Diesel PLIF

Venkat Athmanathan, Matthew Hoeper, Austin M. Webb, Robert B. Wang, Sukesh Roy, H. Douglas Perkins, Christopher A. Fugger and Terrence R. Meyer. "Time resolved visualization of liquid jet interaction with H2-air rotating detonations using MHz rate diesel PLIF," AIAA 2023-0573. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Angle Optimized Filtered Rayleigh Scattering for the Imaging of Pressure Waves from Laser Generated Surface Sparks at 250,000 Frames per Second

James R. Creel, Boris S. Leonov and Richard Miles. "Angle Optimized Filtered Rayleigh Scattering for the Imaging of Pressure Waves from Laser Generated Surface Sparks at 250,000 Frames per Second," AIAA 2023-0350. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Stabilization Effects in Hydromagnetic Plasma Flows

Thomas C. Underwood. "Stabilization Effects in Hydromagnetic Plasma Flows," AIAA 2023-2055. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Simulating Hypervelocity Impacts to High-Density Polyethylene

Jacob Rogers, Paul T. Mead, Justin Wilkerson, Thomas E. Lacy and Neil Williams. "Simulating Hypervelocity Impacts to High-Density Polyethylene," AIAA 2023-2021. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Modes of Laser Spark Ignition of a Model Rocket Combustor

Ryan Strelau, Mark Frederick, Will C. Senior, Rohan Gejji and Carson D. Slabaugh. "Modes of Laser Spark Ignition of a Model Rocket Combustor," AIAA 2023-2377. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

Planar Time-Resolved Laser-Induced Incandescence for Particulate Emissions in Premixed Flames at Elevated Pressures

Andy X. Zheng, Sundar Manikandan, Samuel E. Wonfor, Adam M. Steinberg and Yi C. Mazumdar. "Planar Time-Resolved Laser-Induced Incandescence for Particulate Emissions in Premixed Flames at Elevated Pressures," AIAA 2023-2435. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download

 

High Temperature Gladstone-Dale Coefficient Measurements in a Free-Piston Shock Tube

Gwendolyn Wang, Kyle Daniel, Kyle P. Lynch, Daniel R. Guildenbecher and Yi C. Mazumdar. "High Temperature Gladstone-Dale Coefficient Measurements in a Free-Piston Shock Tube," AIAA 2023-0225. AIAA SCITECH 2023 Forum. January 2023.

Related Industries: High Speed Mechanical Testing and Imaging

Read/Download