UV Accessory Selection Guide for Liquids
Liquid Samples
| Sample | Analytical form and analytical condition | Accessory | |||
|---|---|---|---|---|---|
| Transparent Sample | Sample volume: 2.5 mL min. | Standard Sample Compartment + 10 mm Cell | |||
| Micro-volume measurement | 1 mL min. | Semi-Micro Cell + Micro Cell Holder with Mask | |||
| 500 µL min. | Micro Cell + Micro Cell Holder with Mask | ||||
| 50 µL min. | Super-micro Cell + Super-micro Cell Holder | ||||
| For automatically measuring samples in multiple cells | MMC-1600 8/16 Series Micro Multi-Cell Holders and Cells | ||||
| Samples with high absorbance, but that are difficult to dilute (short optical path measurement) | Short-Path Cell (1, 2, 5 mm) + Spacer for Short-Path Cell | ||||
| Samples with low absorbance, but that are difficult to concentrate (long optical path measurement) | Long-Path Cell (20, 30, 50, 100 mm) + Long-Path Rectangular Cell Holder | ||||
| For automatically measuring samples in multiple cells | Normal measurement | Multi-Cell Sample Compartment (sample volume: 2.5 mL min.) | |||
| Small sample volumes (50 µL min.) | MMC-1600 8/16 Series Micro Multi-Cell Holders and Cells | ||||
| Requires temperature control | CPS-100 Six-Cell Thermoelectrically Temperature-Controlled Cell Positioner (sample volume: 2.5 mL min.) |
||||
| For temperaturecontrolled measurements (constanttemperature measurement) |
Temperature-controlled with water circulation | Constant-Temperature Cell Holder + NTT-2200P Constant-Temperature Water Circulator | |||
| Thermoelectrically temperature controlled | Normal measurement | TCC-100 Thermoelectrically Temperature-Controlled Cell Holder | |||
| Multi Samples | CPS-100 Six-Cell Thermoelectrically Temperature-Controlled Cell Positioner | ||||
| Tm Analysis / Temperature control | S-1700 Thermoelectric Single Cell Holder | ||||
| Automatically supplies sample to flow cells (automatic analysis) |
Requires temperature control (constant-temperature water circulation) | 160C Sipper Unit + NTT-2200P | |||
| Temperature control not necessary | 160L/160T/160U Sipper Unit (Select type based on liquid volume.) | ||||
| Requires accurate control of aspiration volume. | Requires temperature control (constant-temperature water circulation) |
Syringe Sipper CN + NTT-2200P (Select flow cell based on liquid volume.) | |||
| Temperature control not necessary | Syringe Sipper N (Select flow cell based on liquid volume) | ||||
| For automating measurement of multiple samples | Sipper Unit or Syringe Sipper + ASC-5 Auto Sample Changer | ||||
| Suspension Sample | Absorption measurement of suspension samples | Wavelength range: 240 nm min. | Integrating Sphere Attachment (ISR-2600, ISR-2600Plus, ISR-603) | ||
| For measuring UV region above 190 nm | SolidSpec-3700DUV | ||||
| Turbidity measurement | Light transmitted light turbidity measurement (commonly used measurement method) |
10/50 mm Cell + Long-Path Rectangular Cell Holder (Optical path length of cell depends on test method.) |
|||
| Integrating sphere turbidity measurement | Integrating Sphere Attachment (ISR-2600, ISR-2600Plus, ISR-603) | ||||
News / Events
-
SCIX 2025 - The Great SCIentific eXchange (formerly FACSS)
October 6-8
Northern Kentucky Convention Center
Covington, KY
-
Shimadzu Scientific Instruments Introduces Three UV-Vis Spectrophotometers
Shimadzu releases the UV-1900i Plus, UV-2600i Plus, and UV-2700i Plus
-
Shimadzu’s New IRSpirit-X Series of Compact FTIR Spectrophotometers Provide High Performance and Sensitivity in a Space-Saving Design
IRSpirit-X is the smallest and lightest FTIR instrument from Shimadzu with a space-saving design that does not compromise on performance or expandability.
-
New AIMsight Infrared Microscope Maximizes Automation to Improve Microsample Analysis
-
New One-Of-A-Kind AIRsight™ Infrared/Raman Microscope Enables Acquisition of Complementary Molecular Information
-
New IRXross™ FTIR Spectrophotometer Delivers High-End Sensitivity, Enhanced Resolution and High-Quality Data
Shimadzu Scientific Instruments introduces the IRXross™ Fourier Transform Infrared (FTIR) Spectrophotometer. This mid-level FTIR model achieves upper-end performance including high-level S/N ratio, resolution, measurement speed and ease of use.