The UW and UX Series are Shimadzu’s highest performance platform balances. Engineered with the innovative UniBloc one-piece force technology, which provides superior impact resistance and unrivaled response, the UW and UX Series have a wide range of included functions, such as GLP, GMP and ISO calibration reporting, specific gravity measurement, an animal weighing mode, and a formulation mode.

Specifications

UW Model Analytical Balances

Model UW220H UW420H UW620H UW820H UW1020H UW2200H
Capacity 220 g 420 g 620 g 820 g 1.02 kg 2.2 kg
Minimum Display 0.001 g 0.01 g
Repeatability
(standard deviation)
0.001 g 0.01 g
Linearity ±0.002 g ±0.01 g ±0.01 g
Response time 1.5-2.5 secs
UniBloc weighing technology Included
Built-in calibration Included
Built-in clock Included
GLP, GMP and ISO calibration report Included
Analog bar graphic display Included
Specific gravity measurement mode Included
Animal measurement mode Included
Formulation mode Included
Internal timer output Included
Operating temperature range1 5 to 40° C; 30-85% RH
Sensitivity stability against temperature range ±3 ppm/°C (10 to 30°C)
Pan size W X D Approx. 108 x 105 mm Approx. 170 x 180 mm
Body dimensions W x D x H Approx. 190 x 317 x 78 mm
Weight Approx. 3.4 kg Approx. 4.6 kg
Backlight display Included
Input/output terminal RS232
Model UW4200H UW6200H UW420S UW820S UW4200S UW8200S
Capacity 4.2 kg 6.2 kg 420 g 820 g 4.2 kg 8.2 kg
Minimum Display 0.01 g 0.1 g
Repeatability
(standard deviation)
≤0.01 g ≤0.008 g ≤0.08 g
Linearity ±0.02 g ±0.01 g ±0.1 g
Response time 1.5-2.5 secs 0.7-1.2 secs
UniBloc weighing technology Included
Built-in calibration Included
Built-in clock Included
GLP, GMP and ISO calibration report Included
Analog bar graphic display Included
Specific gravity measurement mode Included
Animal measurement mode Included
Formulation mode Included
Internal timer output Included
Operating temperature range1 5 to 40° C; 30-85% RH
Sensitivity stability against temperature range ±3 ppm/°C (10 to 30°C) ±5 ppm/°C (10 to 30°C)
Pan size W X D Approx. 170 x 180 mm Approx. 108 x 105 mm Approx. 170 x 180 mm
Body dimensions W x D x H Approx. 190 x 317 x 78 mm
Weight Approx. 4.6 kg Approx. 3.4 kg Approx. 4.6 kg
Backlight display Included
Input/output terminal RS232

UX Model Analytical Balances

Model UX220H UX420H UX620H UX820H UX1020H UX2200H
Capacity 220 g 420 g 620 g 820 g 1.02 kg 2.2 kg
Minimum Display 0.001 g 0.01 g
Repeatability
(standard deviation)
≤0.001 g ≤0.01 g
Linearity ±0.002 g ±0.003 g ±0.02 g
Response time 1.5-2.5 secs
UniBloc weighing technology Included
Built-in calibration Not available
Built-in clock Included
GLP, GMP and ISO calibration report Included
Analog bar graphic display Included
Specific gravity measurement mode Included
Animal measurement mode Included
Formulation mode Included
Internal timer output Included
Operating temperature range1 5 to 40° C; 30-85% RH
Sensitivity stability against temperature range ±3 ppm/°C (10 to 30°C)
Pan size W X D Approx. 108 x 105 mm Approx. 170 x 180 mm
Body dimensions W x D x H Approx. 190 x 317 x 78 mm
Weight Approx. 2.7 kg Approx. 2.9 kg
Backlight display Included
Input/output terminal RS232
Model UX4200H UX6200H UX420S UX820S UX4200S UX8200S
Capacity 4.2 kg 6.2 kg 420 g 820 g 4.2 kg 8.2 kg
Minimum Display 0.01 g 0.1 g
Repeatability
(standard deviation)
≤0.01 g ≤0.008 g ≤0.1 g
Linearity ±0.02 g ±0.01 g ±0.1 g
Response time 1.5-2.5 secs 0.7-1.2 secs
UniBloc weighing technology Included
Built-in calibration Not available
Built-in clock Included
GLP, GMP and ISO calibration report Included
Analog bar graphic display Included
Specific gravity measurement mode Included
Animal measurement mode Included
Formulation mode Included
Internal timer output Included
Operating temperature range1 5 to 40° C; 30-85% RH
Sensitivity stability against temperature range ±3 ppm/°C (10 to 30°C) ±5 ppm/°C (10 to 30°C)
Pan size W X D Approx. 170 x 180 mm Approx. 108 x 105 mm Approx. 170 x 180 mm
Body dimensions W x D x H Approx. 190 x 317 x 78 mm
Weight Approx. 2.9 kg Approx. 2.7 kg Approx. 2.9 kg
Backlight display Included
Input/output terminal RS232
1. Non-condensing

Installation Space (unit: mm)

UW-UX Series Balance Physical Dimensions

For Research Use Only. Not for use in diagnostic procedures.