Hardware Specifications

Test Frame Range EZ-SX
Test Frame Load Capacity*1 Max. 500N (112 lbs)
Crosshead Speed Range 0.001 to 1000 mm/min
(0.00004 to 39 in/min)
Crosshead Speed Accuracy Within ±0.1% of test speed
Crosshead Positional Accuracy ±0.1% of indicated value or ±0.01mm, whichever is larger
Test Force Measurement Accuracy High-Accuracy Load Cells Within ± 0.5% of indicated test force (for 1/1 to 1/500 of load cell rated capacity)
Standard-Accuracy Load Cells Within ± 1% of indicated test force (for 1/1 to 1/500 of load cell rated capacity)
Depth of Test Space 100 mm (4 in)
Crosshead-Travel 500 mm (19.5 in)
Data Capture Travel 1000 Hz
Standard Input/Output Channels - 1 Dedicated load channel
- 1 Digital input/output channel*2
- 1 Control input/output channel *2

See brochure for more details.

Note 1: When the load cell capacity is smaller than the test frame load capacity, the former is the maximum test force.
Note 2: Optional expansion box can be used to increase the number of channels, see brochure for details.