Hardware Specifications

(UH-X 200KN | UH-X 300KN | UH-FX 300KN | UH-X 500KN | UH-FX 500KN | UH-600KN)

Test Frame Type and Name UH-X
200 kN
UH-X
300 kN
UH-FX
300 kN
UH-X
500 kN
UH-FX
500 kN
UH-X
600 kN
Test Frame Load Capacity Max
200 kN
(44,000 lbs)
Max
300 kN
(67,000 lbs)
Max
300 kN
(67,000 lbs)
Max
500 kN
(112,000 lbs)
Max
500 kN
(112,000 lbs)
Max
600 kN
(134,000 lbs)
Max. Grip Span 800 mm (31 in) 900 mm (35 in)
Max. Compression Plate Span   720 mm (28 in)   800 mm (31 in)
Ram Speed Range 0.1 to 100 mm/min
(0.004 to 3.9 in/min)
0.1 to 80 mm/min
(0.004 to 3 in/min)
Ram Stroke 200 mm (7.8 in) 250 mm (9.8 in)
Effective Table Dimension 500 x 500 mm (19 x 19 in) 650 x 650 mm (25 x 25 in)
Dimensions for Standard Height Test Frame W780 x D500 x H2000
(W31 x D20 x H91 in)
W870 x D520 x H2300
(W35 x D21 x H91 in)
W960 x D650 x H2400
(W38 x D26 x H95 in)
W1060 x D700 x H2400
(W38 x D26 x H95 in)
W960 x D650 x H2400
(W38 x D26 x H95 in)
Weight for Standard Height Test Frame Approximately
900 kg
(1,985 lbs)
Approximately
1,500 kg
(3,306 lbs)
Approximately
1,700 kg
(3,748 lbs)
Approximately
2,600 kg
(5,732 lbs)
Approximately
1,700 kg
(3,748 lbs)
 
 

 
 

Hardware Specifications

(UH-X 1000KN | UH-FX 1000KN | UH-X 2000KN | UH-FX 2000KN)

Test Frame Type and Name UH-X
1000 kN
UH-FX
1000 kN
UH-X
2000 kN
UH-FX
2000 kN
Test Frame Load Capacity Max 1,000 kN
(224,000 lbs)
Max 1,000 kN
(224,000 lbs)
Max 2,000 kN
(449,000 lbs)
Max 2,000 kN
(449,000 lbs)
Max. Grip Span 1,000 mm (39 in) 1,100 mm (43 in)
Max. Compression Plate Span 900 mm (35 in) 950 mm (37 in)
Ram Speed Range 0.1 to 70 mm/min
(0.004 to 2.75 in/min)
0.1 to 50 mm/min
(0.004 to 1.96 in/min)
Ram Stroke 250 mm (9.8 in) 300 mm (11.8 in)
Effective Table Dimension 750 x 750 mm
(29 x 29 in)
850 x 850 mm
(33 x 33 in)
Dimensions for Standard Height Test Frame W1170 x D750 x H2800 mm
(W46 x D30 x H111 in)
W1320 x D800 x H3400 mm
(W52 x D32 x H134 in)
W1560 x D920 x H3400 mm
(W62 x D37 x H134 in)
W1560 x D920 x H4300 mm
(W62 x D37 x H178 in)
 
 
 
 

Hardware Specifications

(UH-X 3000KN | UH-FX 3000KN | UH-X 4000KN | UH-FX 4000KN)

Test Frame Type and Name UH-X
3000 kN
UH-FX
3000 kN
UH-X
4000 kN
UH-FX
4000 kN
Test Frame Load Capacity Max 3,000 kN
(674,000 lbs)
Max 3,000 kN
(674,000 lbs)
Max 4,000 kN
(899,000 lbs)
Max 4,000 kN
(899,000 lbs)
Max. Grip Span 1,200 mm (47 in) 1,400 mm (55 in)
Max. Compression Plate Span 1,000 mm (39 in) 1,150 mm (45 in)
Ram Speed Range 0.1 to 50 mm/min
(0.004 to 1.96 in/min)
Ram Stroke 300 mm (11.8 in) 350 mm (13.7 in)
Effective Table Dimension 1,000 x 1,000 mm
(39 x 39 in)
1,150 x 1,150 mm
(45 x 45 in)
Dimensions for Standard Height Test Frame W1860 x D1100 x H3970 mm
(W74 x D44 x H153 in)
W1860 x D1100 x H5700 mm
(W74 x D44 x H225 in)
W2200 x D1400 x H4800 mm
(W87 x D56 x H189 in)
W2200 x D1400 x H5900 mm
(W87 x D56 x H233 in)
 
 
 
 

UH-X/FX Series Controller Unit

Tester Frame Series UH-X / UH-FX
Test Force Measurement Accuracy Method Cylinder internal pressure measurement with pressure cell
High-Accuracy Load Cells Within ± 0.5% of indicated test force
(for 1/1 to 1/250 of rated capacity)
Standard-Accuracy Load Cells Within ± 1% of indicated test force
(for 1/1 to 1/250 of rated capacity)
 
 
 

Installation Space

UH-X Installation Space Diagram 1

UH-X Installation Space Diagram 2

 

Top of This Page